GBT 12Cr2MoWVTiB

Location » Home » Grades > Special Alloy > 12Cr2MoWVTiB

Grades | Special Alloy | 12Cr2MoWVTiB

GBT 12Cr2MoWVTiB

Print

12Cr2MoWVTiB Application:China structural steel and alloy steel

Chemical composition(mass fraction)(wt.%) of the 12Cr2MoWVTiB
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Mo(%) Ti(%)
0.08-0.15 0.45-0.75 0.45-0.65 0.03 0.03 1.60-2.10 0.50-0.65 0.08-0.18

Mechanical properties of grade 12Cr2MoWVTiB

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
658 (≥) 392 (≥) 32 14 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 314

Physical properties of grade 12Cr2MoWVTiB

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
895 (≥) 765 (≥) 34 12 41 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
688 558 987 - - -

12Cr2MoWVTiB Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED