GBT 30SiMn2MoVA

Location » Home » Grades > Special Alloy > 30SiMn2MoVA

Grades | Special Alloy | 30SiMn2MoVA

GBT 30SiMn2MoVA

Print

30SiMn2MoVA Application:China structural steel and alloy steel

Chemical composition(mass fraction)(wt.%) of the 30SiMn2MoVA
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Ni(%) Mo(%) V(%) Cu(%)
0.27-0.33 0.40-0.60 1.60-1.85 0.025 0.025 Max 0.25 Max 0.25 0.40-0.60 0.15-0.30 Max 0.25

Mechanical properties of grade 30SiMn2MoVA

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
145 (≥) 864 (≥) 24 43 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 341

Physical properties of grade 30SiMn2MoVA

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
829 (≥) 929 (≥) 43 24 33 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
776 749 525 - - -

30SiMn2MoVA Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED