CNS 420J2TKA

Location » Home » Grades > Special Alloy > 420J2TKA

Grades | Special Alloy | 420J2TKA

CNS 420J2TKA

Print

420J2TKA Application:China Taiwan Stainless steel

Chemical composition(mass fraction)(wt.%) of the 420J2TKA
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Ni(%)
0.26-0.40 1.03 1.03 0.04 0.03 12.0-14.0 Max 0.60

Mechanical properties of grade 420J2TKA

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
235 (≥) 582 (≥) 33 33 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 224

Physical properties of grade 420J2TKA

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
237 (≥) 322 (≥) 42 32 11 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
588 698 868 - - -

420J2TKA Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED