CNS CNS 447J1

Location » Home » Grades > Special Alloy > CNS 447J1

Grades | Special Alloy | CNS 447J1

CNS CNS 447J1

Print

CNS 447J1 Application:China Taiwan Stainless steel

Chemical composition(mass fraction)(wt.%) of the CNS 447J1
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Ni(%) Mo(%) N(%) Cu(%) Other(%)
Max 0.010 Max 0.40 Max 0.40 0.03 0.02 28.5-32.0 Max 0.50 1.50-2.50 Max 0.015 Max 0.20 Ni+Cu Max 0.50

Mechanical properties of grade CNS 447J1

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
428 (≥) 399 (≥) 32 11 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 341

Physical properties of grade CNS 447J1

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
177 (≥) 666 (≥) 22 31 41 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
416 243 463 - - -

CNS 447J1 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED