CNS Austenitic 660

Location » Home » Grades > Special Alloy > Austenitic 660

Grades | Special Alloy | Austenitic 660

CNS Austenitic 660

Print

Austenitic 660 Application:China Taiwan Heat-Resistant Steel

Chemical composition(mass fraction)(wt.%) of the Austenitic 660
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Ni(%) Mo(%) V(%) B(%) Al(%) Ti(%)
Max 0.08 Max 1.00 Max 2.00 0.04 0.03 13.5-16.0 24.0-27.0 1.00-1.50 0.10-0.50 0.001-0.010 Max 0.35 1.90-2.35

Mechanical properties of grade Austenitic 660

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
737 (≥) 118 (≥) 21 31 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 122

Physical properties of grade Austenitic 660

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
764 (≥) 273 (≥) 32 14 31 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
321 418 972 - - -

Austenitic 660 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED