CNS SUP3

Location » Home » Grades > Special Alloy > SUP3

Grades | Special Alloy | SUP3

CNS SUP3

Print

SUP3 Application:China Taiwan Structural steel

Chemical composition(mass fraction)(wt.%) of the SUP3
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Mo(%)
0.75-0.90 0.15-0.35 0.30-0.60 0.035 0.035 — —

Mechanical properties of grade SUP3

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
298 (≥) 958 (≥) 11 23 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 343

Physical properties of grade SUP3

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
812 (≥) 471 (≥) 41 23 34 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
686 948 349 - - -

SUP3 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED