CNS S43C

Location » Home » Grades > Special Alloy > S43C

Grades | Special Alloy | S43C

CNS S43C

Print

S43C Application:China Taiwan Structural steel

Chemical composition(mass fraction)(wt.%) of the S43C
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) N(%) Cu(%)
0.40-0.46 0.15-0.35 0.60-0.90 0.030 0.035 0.20 0.20 0.30

Mechanical properties of grade S43C

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
654 (≥) 256 (≥) 41 14 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 123

Physical properties of grade S43C

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
773 (≥) 914 (≥) 22 21 11 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
957 951 534 - - -

S43C Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED