CNS SCM415

Location » Home » Grades > Special Alloy > SCM415

Grades | Special Alloy | SCM415

CNS SCM415

Print

SCM415 Application:China Taiwan Structural steel

Chemical composition(mass fraction)(wt.%) of the SCM415
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Ni(%) Mo(%) Cu(%)
0.13-0.18 0.15-0.35 0.60-0.85 0.030 0.030 0.90-1.20 0.25 0.15-0.30 0.30

Mechanical properties of grade SCM415

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
454 (≥) 762 (≥) 32 43 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 344

Physical properties of grade SCM415

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
972 (≥) 665 (≥) 14 41 21 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
777 595 828 - - -

SCM415 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED