EN EN Fe42B1FN

Location » Home » Grades > Special Alloy > EN Fe42B1FN

Grades | Special Alloy | EN Fe42B1FN

EN EN Fe42B1FN

Print

EN Fe42B1FN Application:Euronorm Structural steel

Chemical composition(mass fraction)(wt.%) of the EN Fe42B1FN
C(%) P(%) S(%)
0.20 0.060 0.050

Mechanical properties of grade EN Fe42B1FN

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
612 (≥) 754 (≥) 12 22 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 134

Physical properties of grade EN Fe42B1FN

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
459 (≥) 267 (≥) 11 13 13 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
293 152 877 - - -

EN Fe42B1FN Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED