EN EN FeH30FU

Location » Home » Grades > Special Alloy > EN FeH30FU

Grades | Special Alloy | EN FeH30FU

EN EN FeH30FU

Print

EN FeH30FU Application:Euronorm Structural steel

Chemical composition(mass fraction)(wt.%) of the EN FeH30FU
C(%) Mn(%) P(%) S(%)
0.08 0.30-0.45 0.025 0.025

Mechanical properties of grade EN FeH30FU

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
876 (≥) 489 (≥) 41 33 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 124

Physical properties of grade EN FeH30FU

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
289 (≥) 276 (≥) 34 21 33 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
334 774 582 - - -

EN FeH30FU Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED