5Cr4Mo3SiMnVA1 Application:Alloy tool steel - hot-work die steel

Chemical composition(mass fraction)(wt.%) of the 5Cr4Mo3SiMnVA1
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Ni(%) Mo(%) V(%) Cu(%) Other(%)
0.47~0.57 0.80~1.10 0.80~1.10 ≤0.030 ≤0.030 3.80~4.30 ≤0.20 2.80~3.40 0.80~1.20 ≤0.30 A1:0.30~0.70

Mechanical properties of grade 5Cr4Mo3SiMnVA1

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
965 (≥) 787 (≥) 42 31 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 414

Physical properties of grade 5Cr4Mo3SiMnVA1

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
149 (≥) 551 (≥) 14 41 22 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
414 759 576 - - -

5Cr4Mo3SiMnVA1 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED