JIS SKS81M

Location » Home » Grades > Special Alloy > SKS81M

Grades | Special Alloy | SKS81M

JIS SKS81M

Print

SKS81M Application:Cold rolled special steel strip

Chemical composition(mass fraction)(wt.%) of the SKS81M
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Ni(%) Cu(%)
1.10-1.30 Max 0.35 Max 0.50 Max 0.030 Max 0.030 0.20~0.50 Max 0.25 Max 0.25

Mechanical properties of grade SKS81M

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
279 (≥) 878 (≥) 23 41 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 421

Physical properties of grade SKS81M

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
212 (≥) 712 (≥) 34 41 23 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
937 786 823 - - -

SKS81M Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED