EN EN X3CrTi17

Location » Home » Grades > Special Alloy > EN X3CrTi17

Grades | Special Alloy | EN X3CrTi17

EN EN X3CrTi17

Print

EN X3CrTi17 Application:Euronorm Stainless Steel

Chemical composition(mass fraction)(wt.%) of the EN X3CrTi17
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Nb(%)
0.050 100 1.00 0*040 0.015 16.0-18.0 4X(C+N)+0.15-0.80

Mechanical properties of grade EN X3CrTi17

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
214 (≥) 943 (≥) 33 34 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 412

Physical properties of grade EN X3CrTi17

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
472 (≥) 385 (≥) 23 32 42 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
552 831 866 - - -

EN X3CrTi17 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED