EN EN X6CrNiMoNb191203KE

Location » Home » Grades > Special Alloy > EN X6CrNiMoNb191203KE

Grades | Special Alloy | EN X6CrNiMoNb191203KE

EN EN X6CrNiMoNb191203KE

Print

EN X6CrNiMoNb191203KE Application:Euronorm Stainless Steel

Chemical composition(mass fraction)(wt.%) of the EN X6CrNiMoNb191203KE
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Ni(%) Mo(%) Cu(%) Nb(%)
0.06 0-55 1.10-1.90 0.025 0.015 18.2-19-8 10.2-12.8 2.60-2.90 0.47 10XCMax 0.95

Mechanical properties of grade EN X6CrNiMoNb191203KE

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
974 (≥) 327 (≥) 23 24 23 Solution and Aging, Annealing, Ausaging, Q+T,etc 121

Physical properties of grade EN X6CrNiMoNb191203KE

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
134 (≥) 323 (≥) 23 23 23 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
427 221 349 - - -

EN X6CrNiMoNb191203KE Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED