EN EN X15CrNiSi25-21

Location » Home » Grades > Special Alloy > EN X15CrNiSi25-21

Grades | Special Alloy | EN X15CrNiSi25-21

EN EN X15CrNiSi25-21

Print

EN X15CrNiSi25-21 Application:Euronorm Stainless Steel

Chemical composition(mass fraction)(wt.%) of the EN X15CrNiSi25-21
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Ni(%)
Max 0.20 1.50-2.50 2.00 0.045 0.015 24.0-25.0 19.0-22.0

Mechanical properties of grade EN X15CrNiSi25-21

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
255 (≥) 194 (≥) 44 31 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 413

Physical properties of grade EN X15CrNiSi25-21

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
283 (≥) 911 (≥) 13 14 21 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
986 622 346 - - -

EN X15CrNiSi25-21 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting