EN X6NiCrTiMoVB25-15-2 Application:Euronorm Stainless Steel

Chemical composition(mass fraction)(wt.%) of the EN X6NiCrTiMoVB25-15-2
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Ni(%) Mo(%) Ti(%)
0.03-0.08 1.00 1.00-2.00 0.025 0.015 13.5-16.0 24.0-27.0 1.00-1.50 1-90-2.30

Mechanical properties of grade EN X6NiCrTiMoVB25-15-2

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
823 (≥) 394 (≥) 23 33 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 312

Physical properties of grade EN X6NiCrTiMoVB25-15-2

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
544 (≥) 737 (≥) 43 43 12 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
577 238 883 - - -

EN X6NiCrTiMoVB25-15-2 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED