EN EN X12CrNiWTiB16-13

Location » Home » Grades > Special Alloy > EN X12CrNiWTiB16-13

Grades | Special Alloy | EN X12CrNiWTiB16-13

EN EN X12CrNiWTiB16-13

Print

EN X12CrNiWTiB16-13 Application:Euronorm Stainless Steel

Chemical composition(mass fraction)(wt.%) of the EN X12CrNiWTiB16-13
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Ni(%) Ti(%)
0.07-0.15 0.50 1.50 0.035 0.015 15.5-17.5 12.5-14.5 0.40-0.70

Mechanical properties of grade EN X12CrNiWTiB16-13

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
769 (≥) 465 (≥) 21 22 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 233

Physical properties of grade EN X12CrNiWTiB16-13

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
312 (≥) 433 (≥) 12 42 24 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
467 584 562 - - -

EN X12CrNiWTiB16-13 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED