GBT GH1016

Location » Home » Grades > Special Alloy > GH1016

Grades | Special Alloy | GH1016

GBT GH1016

Print

GH1016 Application:Solid solution strengthening type iron base alloy

Chemical composition(mass fraction)(wt.%) of the GH1016
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Ni(%) Mo(%) V(%) W(%) N(%) B(%) Nb(%) Other(%)
0.08 0.60 1.80 0.020 0.015 19.0-22.0 32.0-36.0 2.60-3.30 0.10-0.30 5.00-6.00 0.13-0.25 0.01 Max 0.90-1.40 Fe:Balance; Ce≤0.05

Mechanical properties of grade GH1016

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
725 (≥) 538 (≥) 14 13 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 321

Physical properties of grade GH1016

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
848 (≥) 554 (≥) 42 42 43 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
216 718 794 - - -

GH1016 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED