XH60Ю Application:Russia COST standard deformation of high temperature alloy

Chemical composition(mass fraction)(wt.%) of the XH60Ю
C(%) Si(%) Mn(%) Cr(%) Ni(%) Al(%) Other(%)
Max 0.10 Max 0.80 Max 0.30 15.0-18.0 55.0-58.0 2.60-3.50 Ba: Max 0.10,Ce: Max 0.03

Mechanical properties of grade XH60Ю

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
466 (≥) 977 (≥) 11 24 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 233

Physical properties of grade XH60Ю

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
953 (≥) 441 (≥) 12 14 33 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
894 394 554 - - -

XH60Ю Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED