ГОСТ BЖЛ1-BИ

Location » Home » Grades > Special Alloy > BЖЛ1-BИ

Grades | Special Alloy | BЖЛ1-BИ

ГОСТ BЖЛ1-BИ

Print

BЖЛ1-BИ Application:Vacuum melting of casting high temperature alloy rod

Chemical composition(mass fraction)(wt.%) of the BЖЛ1-BИ
C(%) Cr(%) Ni(%) Mo(%) W(%) Al(%) Ti(%)
0.10-0.17 15.0-17.0 Balance 3.5-5.0 2.0-2.5 2.0-2.8 2.0-3.0

Mechanical properties of grade BЖЛ1-BИ

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
214 (≥) 923 (≥) 23 14 23 Solution and Aging, Annealing, Ausaging, Q+T,etc 431

Physical properties of grade BЖЛ1-BИ

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
476 (≥) 617 (≥) 41 11 11 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
681 693 978 - - -

BЖЛ1-BИ Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED