BЖЛ14H-BИ Application:Vacuum melting of casting high temperature alloy rod

Chemical composition(mass fraction)(wt.%) of the BЖЛ14H-BИ
C(%) Cr(%) Ni(%) Mo(%) W(%) Nb(%) Al(%) Ti(%)
0.03-0.08 18.0-20.0 Balance 4.0-5.0   1.8-2.8 1.2-1.5 2.5-2.9

Mechanical properties of grade BЖЛ14H-BИ

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
159 (≥) 793 (≥) 23 11 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 111

Physical properties of grade BЖЛ14H-BИ

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
588 (≥) 556 (≥) 34 43 12 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
827 594 796 - - -

BЖЛ14H-BИ Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED