ГОСТ CДП1-2

Location » Home » Grades > Special Alloy > CДП1-2

Grades | Special Alloy | CДП1-2

ГОСТ CДП1-2

Print

CДП1-2 Application:Standard high temperature oxidation casting alloy rod

Chemical composition(mass fraction)(wt.%) of the CДП1-2
C(%) Si(%) Cr(%) Ni(%) Cu(%) Al(%) Other(%)
Max 0.05 Max 0.2 18-22.00 Balance Max 0.05 11-13.500 0、N、H:Total: 0.02

Mechanical properties of grade CДП1-2

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
394 (≥) 351 (≥) 41 14 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 124

Physical properties of grade CДП1-2

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
593 (≥) 366 (≥) 21 23 33 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
395 147 299 - - -

CДП1-2 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED