Grades | Stainless Steels | CДП1-2

GOST CДП1-2

PDF | Word | Print

CДП1-2 Application:Russia TY standard high temperature oxidation the chemical composition of casting alloy rod

Chemical composition(mass fraction)(wt.%) of the CДП1-2
Elements Min.(≥) Max.(≤) Similar Remarks
Ni - remaining
Co - -
Cr 18.00 22.00
Al 11.00 13.50
Y 0.20 0.60
C - 0.05
Fe - 0.30
Si - 0.20
Cu - 0.05
O、N、H - 0.02

Mechanical properties of grade CДП1-2

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
182 (≥) 611 (≥) 34 41 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 324

Physical properties of grade CДП1-2

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
875 (≥) 397 (≥) 32 24 41 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
796 863 937 - - -

CДП1-2 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED