BD2A

Print

BD2A Application:Carbide for cutting tools

Chemical composition(mass fraction)(wt.%) of the BD2A
C(%) Si(%) Mn(%) Cr(%) Ni(%) Mo(%) V(%) Other(%)
1.60-1.90 ≤0.60 ≤0.60 12.0-13.0 ≤0.40 0.70-0.90 0.25-1.00 Cu≤0.20,Sn≤0.05

Mechanical properties of grade BD2A

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
774 (≥) 475 (≥) 12 23 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 221

Physical properties of grade BD2A

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
833 (≥) 126 (≥) 42 11 24 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
962 653 949 - - -

BD2A Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED