Grades | Structural Steel | 1.7361

DIN 1.7361

PDF | Word | Print

1.7361 Application:Nitriding steel

Chemical composition(mass fraction)(wt.%) of the 1.7361
Elements Min.(≥) Max.(≤) Similar Remarks
C 0.28 0.35
Si - 0.40
Mn 0.40 0.70
P - 0.035
S - 0.035
Cr 2.80 3.30
Mo 0.30 0.50
Ni - 0.60

Mechanical properties of grade 1.7361

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
573 (≥) 173 (≥) 24 31 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 411

Physical properties of grade 1.7361

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
715 (≥) 984 (≥) 41 12 13 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
921 683 837 - - -

1.7361 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED