Grades | Tool Die Steels | T30403

UNS T30403

PDF | Word | Print

T30403 Application:Cold-Work Tool Steel

Chemical composition(mass fraction)(wt.%) of the T30403
Elements Min.(≥) Max.(≤) Similar Remarks
C 2.00 2.35
Si 0.10 0.60
Mn 0.20 0.60
P - 0.030
S - 0.030
Cr 11.00 13.50
Mo - -
V - 1.00
W - 1.00
Ni+Cu - 0.75

Mechanical properties of grade T30403

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
236 (≥) 711 (≥) 42 22 23 Solution and Aging, Annealing, Ausaging, Q+T,etc 312

Physical properties of grade T30403

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
575 (≥) 282 (≥) 42 13 33 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
327 284 626 - - -

T30403 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED