Grades | Tool Die Steels | O6

ASTM O6

PDF | Word | Print

O6 Application:Oil-Hardening Tool Steel

Chemical composition(mass fraction)(wt.%) of the O6
Elements Min.(≥) Max.(≤) Similar Remarks
C 1.25 1.55
Si 0.55 1.50
Mn 0.30 1.10
P - 0.030
S - 0.030
Cr - 0.30
Mo 0.20 0.30
V - -
W - -
Ni+Cu - 0.75

Mechanical properties of grade O6

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
934 (≥) 996 (≥) 42 14 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 124

Physical properties of grade O6

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
353 (≥) 117 (≥) 24 41 43 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
499 461 456 - - -

O6 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED