Grades | Tool Die Steels | T41904

UNS T41904

PDF | Word | Print

T41904 Application:Shock-Resisting Tool Steel

Chemical composition(mass fraction)(wt.%) of the T41904
Elements Min.(≥) Max.(≤) Similar Remarks
C 0.50 0.65
Si 1.75 2.25
Mn 0.60 0.95
P - 0.030
S - 0.030
Cr 0.10 0.50
Mo - -
V 0.15 0.35
W - -
Ni+Cu - 0.75

Mechanical properties of grade T41904

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
756 (≥) 123 (≥) 11 31 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 121

Physical properties of grade T41904

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
341 (≥) 888 (≥) 42 44 11 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
554 882 414 - - -

T41904 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED