Grades | Tool Die Steels | S6

ASTM S6

PDF | Word | Print

S6 Application:Shock-Resisting Tool Steel

Chemical composition(mass fraction)(wt.%) of the S6
Elements Min.(≥) Max.(≤) Similar Remarks
C 0.40 0.50
Si 2.00 2.50
Mn 1.20 1.50
P - 0.030
S - 0.030
Cr 1.20 1.50
Mo 0.30 0.50
V 0.20 0.40
W - -
Ni+Cu - 0.75

Mechanical properties of grade S6

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
219 (≥) 195 (≥) 33 33 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 143

Physical properties of grade S6

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
772 (≥) 171 (≥) 11 42 21 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
143 659 695 - - -

S6 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED