Grades | Tool Die Steels | 75Cr1

DIN 75Cr1

PDF | Word | Print

75Cr1 Application:Tool Steels; Technical Conditions of Delivery

Chemical composition(mass fraction)(wt.%) of the 75Cr1
Elements Min.(≥) Max.(≤) Similar Remarks
C 0.70 0.80
Si 0.25 0.50
Mn 0.60 0.80
P - 0.030
S - 0.030
Cr 0.30 0.40
Mo - -
V - -

Mechanical properties of grade 75Cr1

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
392 (≥) 815 (≥) 42 23 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 112

Physical properties of grade 75Cr1

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
889 (≥) 689 (≥) 11 14 34 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
793 927 281 - - -

75Cr1 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED