Grades | Tool Die Steels | X19NiCrMo4

DIN X19NiCrMo4

PDF | Word | Print

X19NiCrMo4 Application:Tool Steels; Technical Conditions of Delivery

Chemical composition(mass fraction)(wt.%) of the X19NiCrMo4
Elements Min.(≥) Max.(≤) Similar Remarks
C 0.16 0.22
Si 0.10 0.40
Mn 0.15 0.45
P - 0.030
S - 0.030
Cr 1.10 1.40
Mo 0.15 0.25
V - -
Ni 3.80 4.30
W 0.30 0.50

Mechanical properties of grade X19NiCrMo4

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
778 (≥) 115 (≥) 13 12 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 433

Physical properties of grade X19NiCrMo4

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
463 (≥) 444 (≥) 42 21 11 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
124 993 125 - - -

X19NiCrMo4 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED