Grades | Stainless Steels | GH2136

GB GH2136

PDF | Word | Print

GH2136 Application:Classification and designation for superalloys and high temperature intermetallic materials

Chemical composition(mass fraction)(wt.%) of the GH2136
Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.06
Cr 13.0 16.0
Mo 1.00 1.75
Ni 24.5 28.5
Al - 0.35
Ti 2.40 3.20
Si - 0.75
Mn - 0.35
P - 0.025
S - 0.025
B 0.005 0.025
V 0.010 0.1000

Mechanical properties of grade GH2136

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
515 (≥) 178 (≥) 24 31 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 442

Physical properties of grade GH2136

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
626 (≥) 496 (≥) 33 42 42 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
428 388 872 - - -

GH2136 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED