AISI S40800 ( Ferrite )

PDF | Word | Print

S40800 Application:Ferritic Chromium Stainless Steel

Chemical composition(mass fraction)(wt.%) of the S40800
Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.08
Mn - 1.00
Si - 1.00
P - 0.045
S - 0.045
Cr 11.50 13.00
Ni - 0.08
Mo - -

Mechanical properties of grade S40800

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
572 (≥) 919 (≥) 12 33 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 133

Physical properties of grade S40800

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
992 (≥) 744 (≥) 31 32 11 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
651 588 114 - - -

S40800 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED