Grades | Stainless Steels | GH4043

GB GH4043

PDF | Word | Print

GH4043 Application:Classification and designation for superalloys and high temperature intermetallic materials

Chemical composition(mass fraction)(wt.%) of the GH4043
Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.12
Cr 15.0 19.0
Mo 4.00 6.00
Ni - Remainder
W 2.00 3.50
Al 1.00 1.70
Nb 0.50 1.30
Ti 1.90 2.80
Fe - 5.0
Si - 0.60
Mn - 0.50
P - 0.015
S - 0.010
B - 0.01
Ce - 0.03
Co 14.0 16.0

Mechanical properties of grade GH4043

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
627 (≥) 872 (≥) 14 24 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 334

Physical properties of grade GH4043

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
923 (≥) 848 (≥) 32 42 42 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
984 281 423 - - -

GH4043 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED