Grades | Stainless Steels | SA-268 S44800

AMS SA-268 S44800 ( Ferrite )

PDF | Word | Print

SA-268 S44800 Application:Specification for Seamless and Welded Ferritic and Martensitic Stainless Steel Tubing for General Service

Chemical composition(mass fraction)(wt.%) of the SA-268 S44800
Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.01
Mn - 0.30
Si - 0.20
P - 0.025
S - 0.02
Cr 28.00 30.00
Ni 2.00 2.50
Mo 3.50 4.20
N - 0.02
Cu - 0.15

Mechanical properties of grade SA-268 S44800

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
441 (≥) 518 (≥) 14 42 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 132

Physical properties of grade SA-268 S44800

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
435 (≥) 758 (≥) 23 42 24 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
719 149 736 - - -

SA-268 S44800 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED