Grades | Stainless Steels | S20501

AISI S20501 ( Austenite )

PDF | Word | Print

S20501 Application:Stainless steel and heat resistant steel

Chemical composition(mass fraction)(wt.%) of the S20501
Elements Min.(≥) Max.(≤) Similar Remarks
C 0.12 0.25
Si - 1.00
Mn 14.0 15.5
P - 0.06
S - 0.03
Cr 16.5 18.0
Ni 1.00 1.75
N 0.32 0.40

Mechanical properties of grade S20501

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
676 (≥) 552 (≥) 44 13 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 422

Physical properties of grade S20501

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
754 (≥) 358 (≥) 32 14 24 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
772 153 225 - - -

S20501 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED