Grades | Stainless Steels | A 565 S42200

SAE A 565 S42200 ( Martensite )

PDF | Word | Print

A 565 S42200 Application:Martensitic Stainless Steel Bars for High-Temperature Service

Chemical composition(mass fraction)(wt.%) of the A 565 S42200
Elements Min.(≥) Max.(≤) Similar Remarks
C 0.20 0.25
Mn - 1.00
Si - 0.75
P - 0.04
S - 0.03
Cr 11.50 13.50
Ni 0.50 1.00
Mo 0.75 1.25
V 0.15 0.30
W 0.75 1.25

Mechanical properties of grade A 565 S42200

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
619 (≥) 146 (≥) 41 42 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 144

Physical properties of grade A 565 S42200

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
832 (≥) 581 (≥) 21 41 12 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
689 819 956 - - -

A 565 S42200 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED