Grades | Stainless Steels | SA-705 S45500

AMS SA-705 S45500 ( Precipitation-Hardening )

PDF | Word | Print

SA-705 S45500 Application:Specification for Age-Hardening Stainless Steel Forgings

Chemical composition(mass fraction)(wt.%) of the SA-705 S45500
Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.50
Mn - 0.50
Si - 0.50
P - 0.04
S - 0.03
Cr 11.00 12.50
Ni 7.50 9.50
Mo - 0.50

Mechanical properties of grade SA-705 S45500

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
249 (≥) 695 (≥) 23 33 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 322

Physical properties of grade SA-705 S45500

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
765 (≥) 278 (≥) 42 43 23 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
743 146 137 - - -

SA-705 S45500 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED