Grades | Stainless Steels | A 167 S30415

SAE A 167 S30415 ( Austenite )

PDF | Word | Print

A 167 S30415 Application:Stainless and Heat-Resisting Chromium-Nickel Steel Plate, Sheet, and Strip

Chemical composition(mass fraction)(wt.%) of the A 167 S30415
Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.05
Mn - 0.60
Si - 1.30
P - -
S - -
Cr - 18.5
Ni - 9.50
Mo - -
N - 0.15
Ce - 0.04

Mechanical properties of grade A 167 S30415

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
816 (≥) 586 (≥) 31 11 23 Solution and Aging, Annealing, Ausaging, Q+T,etc 311

Physical properties of grade A 167 S30415

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
919 (≥) 841 (≥) 23 31 31 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
485 589 843 - - -

A 167 S30415 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED