Grades | Stainless Steels | SA-240 S30600

AMS SA-240 S30600 ( Austenite )

PDF | Word | Print

SA-240 S30600 Application:Specification for Chromium and Chromium-Nickel Stainless Steel Plate, Sheet, and Strip for Pressure Vessels and for General Applications

Chemical composition(mass fraction)(wt.%) of the SA-240 S30600
Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.018
Mn - 2.00
Si 3.70 4.30
P - 0.02
S - 0.02
Cr 17.00 18.50
Ni 14.00 15.50
Mo - 0.20

Mechanical properties of grade SA-240 S30600

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
979 (≥) 638 (≥) 22 11 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 311

Physical properties of grade SA-240 S30600

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
598 (≥) 629 (≥) 43 22 14 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
582 743 923 - - -

SA-240 S30600 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED