Grades | Stainless Steels | B 709 N08028

SAE B 709 N08028 ( Austenite )

PDF | Word | Print

B 709 N08028 Application:Iron-Nickel-Chromium-Molybdenum Alloy (UNS N08028)* Plate, Sheet, and Strip

Chemical composition(mass fraction)(wt.%) of the B 709 N08028
Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.02
Mn - 2.00
Si - 1.00
P - 0.02
S - 0.015
Cr 26.00 28.00
Ni 29.50 32.50
Mo 3.00 4.00
Cu 0.60 1.40

Mechanical properties of grade B 709 N08028

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
416 (≥) 865 (≥) 44 12 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 412

Physical properties of grade B 709 N08028

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
846 (≥) 932 (≥) 24 44 41 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
826 328 347 - - -

B 709 N08028 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED