AMS SA-312 Grade TP XM-11 ( Austenite )

PDF | Word | Print

SA-312 Grade TP XM-11 Application:Specification for Seamless and Welded Austenitic Stainless Steel Pipes

Chemical composition(mass fraction)(wt.%) of the SA-312 Grade TP XM-11
Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.04
Si - 1.00
Mn 8.00 10.0
P - 0.06
S - 0.03
Cr 19.0 21.5
Ni 5.50 7.50
N 0.15 0.40

Mechanical properties of grade SA-312 Grade TP XM-11

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
343 (≥) 591 (≥) 34 33 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 123

Physical properties of grade SA-312 Grade TP XM-11

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
229 (≥) 922 (≥) 43 32 44 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
873 236 181 - - -

SA-312 Grade TP XM-11 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting