Grades | Stainless Steels | 15-5PH

ASTM 15-5PH

PDF | Word | Print

15-5PH Application:High temperature alloys and other special alloys

Chemical composition(mass fraction)(wt.%) of the 15-5PH
Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.07
Si - -
Mn - -
Cr 14.0 15.5
Ni 3.5 5.5
Cu 2.5 4.5

Mechanical properties of grade 15-5PH

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
327 (≥) 642 (≥) 13 42 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 233

Physical properties of grade 15-5PH

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
572 (≥) 263 (≥) 43 34 12 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
192 787 953 - - -

15-5PH Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED