Grades | Stainless Steels | SB-462 N06025
AMS SB-462 N06025 ( Precipitation-Hardening )
PDF | Word | Print
SB-462 N06025 Application:Standard Specification for Forged or Rolled UNS N06030, UNS N06022, UNS N06035, UNS N06200, UNS N06059, UNS N10362, UNS N06686, UNS N08020, UNS N08024, UNS N08026, UNS N08367, UNS N10276, UNS N10665, UNS N10675, UNS N10629, UNS N08031, UNS N06045
| Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
|---|---|---|---|---|
| C | - | 0.01 | ||
| Si | - | 0.05 | ||
| Mn | - | 1.50 | ||
| P | - | 0.04 | ||
| S | - | 0.01 | ||
| Ni | - | remaining | ||
| Cr | 0.50 | 1.50 | ||
| Al | 0.10 | 0.50 | ||
| Cu | - | 0.50 | ||
| Ti | - | - | ||
| Fe | 1.00 | 6.00 | ||
| Mo | 26.00 | 30.00 | ||
| Co | - | 2.50 |
| Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | HBW |
|---|---|---|---|---|---|---|
| 874 (≥) | 264 (≥) | 34 | 24 | 11 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 414 |
| Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
|---|---|---|---|---|---|
| 793 (≥) | 479 (≥) | 12 | 11 | 31 | Solution and Aging, Annealing, Ausaging, Q+T,etc |
| Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
- | - | - |
| 666 | 699 | 734 | - | - | - |
| Product type | Products | Dimension | Processes | Deliver Status |
|---|---|---|---|---|
| Plates / Sheets | Plates / Sheets | 0.08-200mm(T)*W*L | Forging, hot rolling and cold rolling | Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting |
| Steel Bar | Round Bar, Flat Bar, Square Bar | Φ8-1200mm*L | Forging, hot rolling and cold rolling, Cast | Black, Rough Turning, Shot Blasting, |
| Coil / Strip | Steel Coil /Steel Strip | 0.03-16.0x1200mm | Cold-Rolled & Hot-Rolled | Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting |
| Pipes / Tubes | Seamless Pipes/Tubes, Welded Pipes/Tubes | OD:6-219mm x WT:0.5-20.0mm | Hot extrusion, Cold Drawn, Welded | Annealed, Solution and Aging, Q+T, ACID-WASHED |