Kovar Application:Iron-Nickel-Cobalt Alloy, Bars and Forgings, 53Fe - 29Ni - 17Co, Low Expansion, Glass Sealing

Chemical composition(mass fraction)(wt.%) of the Kovar
Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.04
Si - 0.20
Mn - 0.50
Ni - 29.00
Cr - 0.20
Al - 0.10
Cu - 0.20
Ti - 0.10
Fe - 53.00
Mo - 0.20
Co - 17.00
W - -
Mg - 0.10
Zr - 0.10

Mechanical properties of grade Kovar

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
978 (≥) 668 (≥) 21 31 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 214

Physical properties of grade Kovar

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
145 (≥) 711 (≥) 21 13 42 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
185 334 539 - - -

Kovar Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED