Grades | Stainless Steels | SUS 410 TKA

JIS SUS 410 TKA ( Martensite )

PDF | Word | Print

SUS 410 TKA Application:Stainless steel pipes for machine and structural purposes

Chemical composition(mass fraction)(wt.%) of the SUS 410 TKA
Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.15
Si - 1.00
Mn - 1.00
P - 0.04
S - 0.03
Cr 11.50 13.50
Ni - 0.60
Mo - -
N - -

Mechanical properties of grade SUS 410 TKA

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
615 (≥) 264 (≥) 34 14 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 443

Physical properties of grade SUS 410 TKA

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
514 (≥) 934 (≥) 44 32 24 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
554 277 984 - - -

SUS 410 TKA Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED