JIS SUH 35 ( Martensite )

PDF | Word | Print

SUH 35 Application:Heat-resisting steel bars and wire rods

Chemical composition(mass fraction)(wt.%) of the SUH 35
Elements Min.(≥) Max.(≤) Similar Remarks
C 0.35 0.45
Si 1.80 2.50
Mn - 0.60
P - 0.03
S - 0.03
Cr 10.00 12.00
Ni - 0.60
Mo 0.70 1.30

Mechanical properties of grade SUH 35

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
735 (≥) 855 (≥) 31 31 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 333

Physical properties of grade SUH 35

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
651 (≥) 963 (≥) 44 43 23 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
165 544 151 - - -

SUH 35 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED