Grades | Stainless Steels | NCF 718

JIS NCF 718

PDF | Word | Print

NCF 718 Application:Corrosion-resisting and heat-resisting superalloy plates and sheets

Chemical composition(mass fraction)(wt.%) of the NCF 718
Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.08
Si - 0.35
Mn - 0.35
P - 0.015
S - 0.015
Cr 17.00 21.00
Ni 50.00 55.00
Cu - 0.30
Al 0.20 0.80
Ti 0.65 1.15
Fe remaining -
Nb+Ta 4.75 5.50
Mo 2.80 3.30
B - 0.006

Mechanical properties of grade NCF 718

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
883 (≥) 134 (≥) 11 24 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 332

Physical properties of grade NCF 718

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
792 (≥) 789 (≥) 42 31 44 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
869 683 578 - - -

NCF 718 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED