Grades | Stainless Steels | HFS304 S51

B.S. HFS304 S51

PDF | Word | Print

HFS304 S51 Application:Austenitic stainless steel pipes and tubes for pressure purposes. Specification for seamless tubes

Chemical composition(mass fraction)(wt.%) of the HFS304 S51
Elements Min.(≥) Max.(≤) Similar Remarks
C 0.04 0.10
Si - 1.00
Mn - 2.00
P - 0.045
S - 0.025
Cr 17.00 19.00
Mo - -
Ni 8.00 11.00

Mechanical properties of grade HFS304 S51

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
218 (≥) 463 (≥) 12 33 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 343

Physical properties of grade HFS304 S51

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
361 (≥) 613 (≥) 43 33 21 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
693 377 323 - - -

HFS304 S51 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED