Grades | Stainless Steels | HR203

B.S. HR203

PDF | Word | Print

HR203 Application:Specification for nickel-chromium-titanium heat-resisting alloy plate, sheet and strip (nickel base, Cr 19.5, Ti 0.4)

Chemical composition(mass fraction)(wt.%) of the HR203
Elements Min.(≥) Max.(≤) Similar Remarks
C 0.08 0.15
Si - 1.00
Mn - 1.00
P - -
S - 0.020
Cr 18.00 21.00
Ni - remaining
Mo - -
Co - 0.50
Ti 0.20 0.60
Fe - 5.00
Cu - 0.50
Pb - 0.005

Mechanical properties of grade HR203

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
291 (≥) 278 (≥) 12 34 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 114

Physical properties of grade HR203

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
254 (≥) 828 (≥) 21 13 33 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
713 631 529 - - -

HR203 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED